dc.description.abstract2,5-Dihydro-2,5-dimethoxyfuran (DHMF) was polymerized via constant current electrolysis (CCE), in CH3CN-NaClO4 solvent-electrolyte couple. Poly(DHMF) was obtained from the anolyte. The effect of current density, temperature, monomer and electrolyte concentrations on the polymer yield have been examined. The apparent activation energy for CCE of DHMF was found to be 37.2 kJ/mol. The FTIR and H-1-NMR analyses show that DHMF polymerizes by a ring opening. Molecular weight of poly(DHMF) was found by using cryoscopy.en_US
dc.identifier.citationclosedAccessen_US
dc.identifier.doi10.1007/s00289-004-0246-4
dc.identifier.endpage40en_US
dc.identifier.issn0170-0839
dc.identifier.issn1436-2449
dc.identifier.issue1en_US
dc.identifier.scopus2-s2.0-3042823818
dc.identifier.scopusqualityQ1
dc.identifier.startpage33en_US
dc.identifier.urihttps://doi.org/10.1007/s00289-004-0246-4
dc.identifier.urihttps://hdl.handle.net/20.500.12587/3293
dc.identifier.volume52en_US
dc.identifier.wosWOS:000222239200005
dc.identifier.wosqualityQ2
dc.indekslendigikaynakWeb of Science
dc.indekslendigikaynakScopus
dc.language.isoen
dc.publisherSpringeren_US
dc.relation.ispartofPolymer Bulletin
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US
dc.rightsinfo:eu-repo/semantics/closedAccessen_US
dc.titleRing opening polymerization of 2,5-dihydro-2,5-dimethoxyfuran by electrochemical initiationen_US
dc.typeArticle

Dosyalar

Orijinal paket
Listeleniyor 1 - 1 / 1
[ X ]
İsim:
Ring opening polymerization of 2,5-dihydro-2,5-dimethoxyfuran by electrochemical initiation.pdf
Boyut:
348.06 KB
Biçim:
Adobe Portable Document Format
Açıklama:
Tam Metin/Full Text