dc.description.abstract | Statement of problem. Surface treatment methods used for resin bonding to conventional silica-based dental ceramics are not reliable for zirconium-oxide ceramics. Purpose. The aim of this study was to compare the effects of airborne-particle abrasion, silanization, tribochemical silica coating, and a combination of bonding/silane coupling agent surface treatment methods on the bond strength of zirconium-oxide ceramic to a resin luting agent. Material and methods. Sixty square-shaped (5 X 5 X 1.5 mm) zirconium-oxide ceramic (Cercon) specimens and composite resin (Z-250) cylinders (3 X 3 mm) were prepared. The ceramic surfaces were airborne-particle abraded with 125-mu m aluminum-oxide (Al2O3) particles and then divided into 6 groups (n=10) that were subsequently treated as follows: Group C, no treatment (control); Group SIL, silanized with a silane coupling agent (Clearfil Porcelain Bond Activator); Group BSIL, application of the adhesive 10-methacryloyloxydecyl dihydrogen phosphate monomer (MDP)-containing bonding/silane coupling agent mixture (Clearfil Liner Bond 2V/Porcelain Bond Activator); Group SC, silica coating using 30-mu m Al2O3 particles modified by silica (CoJet System); Group SCSIL, silica coating and silanization (CoJet System); and Group SCBSIL, silica coating and application of an MDP-containing bonding/silane coupling agent mixture (Clearfil Liner Bond 2V/Porcclain Bond Activator). The composite resin cylinders were bonded to the treated ceramic surfaces using an adhesive phosphate monomer-containing resin luting agent (Panavia F). After the specimens were stored in distilled water at 37 degrees C for 24 hours, their shear bonding strength was tested using a universal testing machine at a crosshead speed of 0.5 mm/min. Debonded specimen surfaces were examined with a stereomicroscope to assess the mode of failure, and the treated surfaces were observed by scanning electron microscopy. Bond strength data were analyzed using 1-way analysis of variance and the Duncan test (alpha=.05). Results. The bond strengths (mean +/- SD; MPa) in the groups were as follows: Group C, 15.7 +/- 2.9; Group SIL, 16.5 +/- 3.4; Group BSIL, 18.8 +/- 2.8; Group SC, 21.6 +/- 3.6; Group SCSIL, 21.9 +/- 3.9; and Group SCBSIL, 22.9 +/- 3.1. The bond strength was significantly higher in Group SCBSIL than in Groups C, SIL, and BSIL (P<.001), but did not differ significantly from those in Groups SC and SCSIL. Failure modes were primarily adhesive at the interface between zirconium and the resin luting agent in Groups C and SIL, and primarily mixed and cohesive in Groups SC, SCSIL, and SCBSIL. Conclusion. Tribochemical silica coating (CoJet System) and the application of an MDP-containing bonding/silane coupling agent mixture increased the shear bond strength between zirconium-oxide ceramic and resin luting agent (Panavia F). | en_US |
dc.identifier.citation | closedAccess | en_US |
dc.identifier.doi | 10.1016/j.prosdent.2006.03.016 | |
dc.identifier.endpage | 436 | en_US |
dc.identifier.issn | 0022-3913 | |
dc.identifier.issn | 1097-6841 | |
dc.identifier.issue | 6 | en_US |
dc.identifier.pmid | 16765155 | |
dc.identifier.scopus | 2-s2.0-33744789998 | |
dc.identifier.scopusquality | Q1 | |
dc.identifier.startpage | 430 | en_US |
dc.identifier.uri | https://doi.org10.1016/j.prosdent.2006.03.016 | |
dc.identifier.uri | https://hdl.handle.net/20.500.12587/3781 | |
dc.identifier.volume | 95 | en_US |
dc.identifier.wos | WOS:000238395200007 | |
dc.identifier.wosquality | Q3 | |
dc.indekslendigikaynak | Web of Science | |
dc.indekslendigikaynak | Scopus | |
dc.indekslendigikaynak | PubMed | |
dc.language.iso | en | |
dc.publisher | Mosby-Elsevier | en_US |
dc.relation.ispartof | Journal Of Prosthetic Dentistry | |
dc.relation.publicationcategory | Makale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı | en_US |
dc.rights | info:eu-repo/semantics/closedAccess | en_US |
dc.title | Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin | en_US |
dc.type | Article |
Dosyalar
Orijinal paket
1 - 1 / 1
[ X ]
- İsim:
- Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin.pdf
- Boyut:
- 408.18 KB
- Biçim:
- Adobe Portable Document Format
- Açıklama:
- Tam Metin/Full Text