Sintering and Characterization of SiC Reinforced Ni Powders in Microwave Furnace
[ X ]
Tarih
2020
Yazarlar
Dergi Başlığı
Dergi ISSN
Cilt Başlığı
Yayıncı
Kırıkkale Üniversitesi
Erişim Hakkı
info:eu-repo/semantics/openAccess
Özet
SiC reinforced nickel matrix composites,microwave at different temperatures It is produced by sintering in oven. Nickeldeposition on SiC powders was achieved by using electroless nickel platingtechnique. It is sintered at temperaturesbetween 500°C, 600 °C, 700°C, 800°C and 900°C under Ar atmosphere. XRD, SEM(Scanning Electron Microscope), pressure test and hardness measurements wereused to characterize the properties of sintered samples in microwave furnace. Theexperimental results, maximum compressive strength (?max) and hardness (HV)were carried out at 800 °C. Microwavesintering of Ni-coated SiC powders without electric current can be a promisingtechnique for producing ceramic-reinforced nickel composites.
Açıklama
Anahtar Kelimeler
Microwave sintering, Powder metallurgy, Composites, Nickel plating
Kaynak
Uluslararası Mühendislik Araştırma ve Geliştirme Dergisi
WoS Q Değeri
Scopus Q Değeri
Cilt
1
Sayı
1-83