Sintering and Characterization of SiC Reinforced Ni Powders in Microwave Furnace

dc.contributor.authorYonetken, Ahmet
dc.contributor.authorErol, Ayhan
dc.date.accessioned2025-01-21T14:28:47Z
dc.date.available2025-01-21T14:28:47Z
dc.date.issued2020
dc.description.abstractSiC reinforced nickel matrix composites,microwave at different temperatures It is produced by sintering in oven. Nickeldeposition on SiC powders was achieved by using electroless nickel platingtechnique.  It is sintered at temperaturesbetween 500°C, 600 °C, 700°C, 800°C and 900°C under Ar atmosphere. XRD, SEM(Scanning Electron Microscope), pressure test and hardness measurements wereused to characterize the properties of sintered samples in microwave furnace. Theexperimental results, maximum compressive strength (?max) and hardness (HV)were carried out at 800 °C.  Microwavesintering of Ni-coated SiC powders without electric current can be a promisingtechnique for producing ceramic-reinforced nickel composites.
dc.identifier.dergipark474003
dc.identifier.doi10.29137/umagd.474003
dc.identifier.issn1308-5514
dc.identifier.issue1-83
dc.identifier.startpage89
dc.identifier.urihttps://dergipark.org.tr/tr/download/article-file/947747
dc.identifier.urihttps://dergipark.org.tr/tr/pub/umagd/issue/49089/474003
dc.identifier.urihttps://doi.org/10.29137/umagd.474003
dc.identifier.urihttps://hdl.handle.net/20.500.12587/20358
dc.identifier.volume1
dc.language.isoen
dc.publisherKırıkkale Üniversitesi
dc.relation.ispartofUluslararası Mühendislik Araştırma ve Geliştirme Dergisi
dc.relation.publicationcategoryMakale - Ulusal Hakemli Dergi
dc.rightsinfo:eu-repo/semantics/openAccess
dc.snmzKA_20241229
dc.subjectMicrowave sintering
dc.subjectPowder metallurgy
dc.subjectComposites
dc.subjectNickel plating
dc.titleSintering and Characterization of SiC Reinforced Ni Powders in Microwave Furnace