Özet

In this study, it is investigated that are calcite filler can be used in the production of medium density fiberboard. Chips have been to the process of cooking for 4-5 minutes in Asplund defibrator with the vapor pressure of 7-7.5 bar, and 1800C temperature. 1.5% paraffin and 1% ammonium sulphate to be pulverized is added to fibers on the output of defibrillator and blowline line. Calcite fillers are prepared in a separate tank in order to use calcite instead of lignocellulosic fibers in the production of 1 m(3) MDF. After that, urea formaldehyde glue is prepared as three different solutions which include the calcite, respectively with 3% (20 kgm(-3)), 6% (40 kg-m(-3)), 9% (60 kg-m(-3)). The fibers are dried to moisture of 8%-12%. This press applies temperature about 185-190 degrees C and pressure about 32-34 kg-m(-2) to the mixture material for 270 seconds during pressing time. MDF panels (2100 x 4900 x 18 mm) were produced in the process. Both mechanical and physical experiments are performed on boards which are produced.

Açıklama

Anahtar Kelimeler

MDF, fiberboard, calcite filler, physical properties, mechanical properties

Kaynak

WOOD RESEARCH

WoS Q Değeri

Q3

Scopus Q Değeri

Q2

Cilt

65

Sayı

2

Künye

Bu makale açık erişimli değildir.